Kayayyaki
Extruder Parallel Twin Screw
  • Extruder Parallel Twin ScrewExtruder Parallel Twin Screw

Extruder Parallel Twin Screw

Injiniya don tsawon rai da ingantaccen inganci, Nanhaiya's Extruder Parallel Twin Screws yana ba da garantin ingantaccen tsarin samarwa da isar da ingantaccen samfur. Ana amfani da su sosai wajen fitar da robobi da robobi, da kuma sarrafa polymers kamar su PVC, PE, PP, da ƙari. Bugu da ƙari, suna samun aikace-aikace a cikin haɗawa, granulation, da kuma samar da kayan aiki mai girma.

Extruder Parallel Twin Screw - Babban inganci da ɗorewa tagwaye sukurori don PVC, PE, PP, da LDPE extrusion. Abubuwan da za'a iya daidaita su suna tabbatar da yumɓu mai yumɓu, ingantaccen fitarwa, da ingantaccen samfur don fim, bututu, bayanin martaba, da samar da pellet.

Sigar Samfur (Takaddamawa)

Kayan abu

38CrMoAlA

Taurin Maganin Zafi

HB260-320

Nitriding Hardness

HV950-1000

Zurfin Nitriding

0.50-0.70mm

Nitriding Brittleness

≤ Darasi 1

Tashin hankali

Ra 0.4

Matsakaicin Madaidaici

0.015mm

Chrome Plating Hardness

HV≥950HV

Kauri Chrome

0.05-0.10mm

Taurin Bimetal

Saukewa: HRC60-65

Zurfin Bimetal

2.0-3.0mm

Siffar Samfurin da Aikace-aikace

Mafi dacewa don PVC, PE, PP, LDPE, da robobi da aka gyara, nau'ikan tagwayen mu masu kama da juna suna ba da kayan filastik iri ɗaya, ingantaccen hadawa, da tsayayyen extrusion, wanda ke haifar da inganci mai inganci, pellets na gaskiya. Cikakke don layin extrusion mai sauri, suna haɓaka yawan aiki yayin rage yawan kuzari. Ana amfani da waɗannan sukurori sosai a cikin fim, bututu, bayanin martaba, da samar da pellet, da kuma a cikin masterbatch, cike da robobi, da sauran kayayyaki na musamman.

Mu Extruder Parallel Twin sukurori ana amfani da ko'ina a aikace-aikace kamar fim extrusion, bututu da profile samar, da pelletizing. Hakanan sun dace da samar da pellet na zahiri, masterbatches, da robobi da aka cika, suna mai da su kyakkyawan zaɓi don masana'antu kamar sarrafa filastik, kayan gini, da marufi.

Extruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin Screw

Cikakken Bayani

Nanhaiya Extruder Parallel Twin Screws an ƙera su daga karfe 38CrMoAlA nitrided don haɓaka juriya, juriya, da ƙarfi. Cikakken customizable da kayan zažužžukan kamar zafi aiki karfe, sanyi aikin karfe, high-gudun karfe, HIP foda karfe, da kuma PTA gami, wadannan sukurori an tsara don ingantaccen plasticizing, uniform hadawa, da kuma barga extrusion.

Cikakke don PVC, PE, PP, LDPE, da robobi da aka gyara, ana amfani da su sosai a cikin samar da pellet, fim, bututu, da haɓaka bayanan martaba. Waɗannan sukurori sun dace don samar da masterbatch, robobi da aka cika, da kayan aiki. Tare da nau'ikan diamita daban-daban da ma'aunin L / D da ke akwai, kamar 65/33, 65/38, da 80/156, an inganta su don manyan layukan extrusion masu saurin gaske, suna ba da ingantaccen makamashi da tsayin daka don daidaiton aiki da rage raguwar lokaci.

Extruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin ScrewExtruder Parallel Twin Screw
Aika tambaya
Bayanan Tuntuɓi
Barka da zuwa gidan yanar gizon mu! Don tambayoyi game da samfuranmu ko lissafin farashi, da fatan za a bar mana imel ɗin ku kuma za mu kasance cikin tuntuɓar sa'o'i 24.
X
Muna amfani da kukis don ba ku ingantaccen ƙwarewar bincike, bincika zirga-zirgar rukunin yanar gizo da keɓance abun ciki. Ta amfani da wannan rukunin yanar gizon, kun yarda da amfaninmu na kukis. takardar kebantawa
ƘiKarba