Kayayyaki

Madaidaicin Injection Molding Screw don Injin allurar Filastik

Samfuran gyare-gyaren allura da aka saba amfani da su:

Adadin allura
(g)

Tsawon Diamita X
(mm)

Ganga Diamita X Tsawon
(mm)

Adadin allura
(g)

Tsawon Diamita X
(mm)

Ganga Diamita X Tsawon
(mm)

30-90

Φ30x900

Φ85x860

80-125

Φ75x1825

Φ170x1725

60-125

Φ35x910

Φ85x860

100-150

Φ80x2000

Φ180x1805

100-150

Φ38x935

Φ95x900

125-200

Φ85x2300

Φ190x1900

125-160

Φ40x980

Φ95x910

200-300

Φ90x2700

Φ210x2000

125-300

Φ42x1030

Saukewa: 105X1110

250-500

Φ100x2600

Φ230x2405

250-400

Φ45x1210

Φ115x1165

300-600

Φ110x2600

Φ256x2590

300-500

Φ50x1300

Φ125x1260

400-1000

Φ120x2800

Φ256x2800

450-600

Φ55x1335

Φ130x1320

600-800

Φ130x3010

Φ256x2970

500-700

Φ56x1350

Φ130x1350

800-1000

Φ145x3010

Φ256x3200

500-700

Φ60x1380

Φ140x1350

1000-1500

Φ160x3500

Φ270x3200

650-800

Φ65x1415

Φ150x1420

1300-2500

Φ170x3415

Φ317X3380

700-1000

Φ70x1790

Φ160x1685

 

 



NanhaiyaAn yi sukukulan gyare-gyaren allura da karfe 38CrMoALA, wanda aka yi da zafi, wanda ya dace da sarrafa robobi marasa lalacewa kamar PE da PP, tare da rayuwar sabis na kusan awanni 10,000-20,000. Bayan quenching da tempering, juriya lalacewa ya karu da 50%, sa su dace da sarrafa ƙarfafa robobi dauke da gilashin fiber (≤30%) (kamar PA + gilashin fiber). Mun nitrid da allura gyare-gyaren sukurori, yin gas nitriding a 500-560 ℃ don samar da wani nitrided Layer da kauri na 0.5-0.8mm (taurin 950-1050HV), wanda zai iya inganta lalacewa juriya da 30% -40%.


Za a iya amfani da kusoshi masu gyare-gyaren allura don:PE, PP, PS, ABS. Aikace-aikace sun haɗa da: kayan aikin bututu na PVC, ƙofar filastik da kayan haɗin taga; PA na gefen injin ingin; PBT LED fitilu masu riƙe da wutar lantarki; da gilashin fiber ƙarfafa PA da carbon fiber ƙarfafa kayan PC.


View as  
 
Mutant Injection Molding Screw

Mutant Injection Molding Screw

Zhoushan Nanhaiya Plastic Machinery Co., Ltd. is one of the earliest professional manufacturers in China specializing in Mutant Injection Molding Screw and barrels for sol-gel molding machines. Tare da fiye da shekaru goma na gwaninta a cikin injunan robobi, samfuran mu masu inganci, daidaitattun kayan aikin injiniya sun sami amincewar abokan ciniki a duk duniya. Mafi girman farashin mu na mutatattun alluran gyare-gyaren gyare-gyaren gyare-gyaren mu yana kaiwa kasuwanni daban-daban. Muna fatan zama abokin tarayya na dogon lokaci a kasar Sin.
A hankali Allura Molding Screw

A hankali Allura Molding Screw

Zhoushan Nanhaiya Plastic Machinery Co., Ltd. yana ɗaya daga cikin ƙwararrun masana'antun masana'antu na farko a kasar Sin wanda ya ƙware a kan ingantattun sukurori da ganga don injunan gyare-gyaren sol-gel. Tare da fiye da shekaru goma na gwaninta a cikin injunan robobi, samfuran mu masu inganci, daidaitattun kayan aikin injiniya sun sami amincewar abokan ciniki a duk duniya. Mafi kyawun farashin mu don dunƙule alluran gyare-gyaren mu a hankali yana kaiwa kasuwanni daban-daban. Muna fatan zama abokin tarayya na dogon lokaci a kasar Sin.